您的位置:網(wǎng)站首頁(yè)>
技術(shù)論文

激發(fā)劑對(duì)粉煤灰水泥膠凝材料水化性能的影
發(fā)布時(shí)間: 2006-04-01 00:00 查看: 2688次
蔣林華 林寶玉 蔡躍波 夏頌佑
摘要:用結(jié)合水量、三甲基硅烷化―氣相色譜、差熱分析和X射線衍射等方法研究了激發(fā)劑對(duì)粉煤灰水泥膠凝材料水化性能的影響,發(fā)現(xiàn)激發(fā)劑能加快粉煤灰水泥膠凝材料的水化速度,使粉煤灰先解聚再水化.粉煤灰中單摻激發(fā)劑,水化反映難以進(jìn)行.激發(fā)劑對(duì)粉煤灰水泥膠凝材料的水化產(chǎn)物種類影響不大.
關(guān)鍵詞:粉煤灰;水泥;激發(fā)劑;水化性能
分類號(hào):TQ172.1+4 文獻(xiàn)標(biāo)識(shí)碼:A
文章編號(hào):1000-1980(2000)03-0095-04
Effects of Activator on the Hydration Properties
of Fly Ash-Cement Binders
JIANG Lin-hua
(College of Civil Engineering, Hohai Univ., Nanjing 210098, China)
LIN Bao-yu CAI Yuebo
(Nanjing Hydraulic Research Institute, Nanjing 210024,China)
XIA Song-you
(College of Water Conservancy and Hydropower Engineering, Hohai Univ.,Nanjing 210098,China)
Abstract:The effects of activator on the hydration properties of fly ash-cement binders are studied by use of bound water, TMS-GC, DTA and XRD. It is found that the hydration of fly ash-cement binders is accelerated by activator and fly ash is depolymerized prior to hydration. The hydration of fly ash is difficult by adding activator alone. The activator has little effect on the kinds of hydration products.
Key words:fly ash;cement;activator;hydration properties
摘要:用結(jié)合水量、三甲基硅烷化―氣相色譜、差熱分析和X射線衍射等方法研究了激發(fā)劑對(duì)粉煤灰水泥膠凝材料水化性能的影響,發(fā)現(xiàn)激發(fā)劑能加快粉煤灰水泥膠凝材料的水化速度,使粉煤灰先解聚再水化.粉煤灰中單摻激發(fā)劑,水化反映難以進(jìn)行.激發(fā)劑對(duì)粉煤灰水泥膠凝材料的水化產(chǎn)物種類影響不大.
關(guān)鍵詞:粉煤灰;水泥;激發(fā)劑;水化性能
分類號(hào):TQ172.1+4 文獻(xiàn)標(biāo)識(shí)碼:A
文章編號(hào):1000-1980(2000)03-0095-04
Effects of Activator on the Hydration Properties
of Fly Ash-Cement Binders
JIANG Lin-hua
(College of Civil Engineering, Hohai Univ., Nanjing 210098, China)
LIN Bao-yu CAI Yuebo
(Nanjing Hydraulic Research Institute, Nanjing 210024,China)
XIA Song-you
(College of Water Conservancy and Hydropower Engineering, Hohai Univ.,Nanjing 210098,China)
Abstract:The effects of activator on the hydration properties of fly ash-cement binders are studied by use of bound water, TMS-GC, DTA and XRD. It is found that the hydration of fly ash-cement binders is accelerated by activator and fly ash is depolymerized prior to hydration. The hydration of fly ash is difficult by adding activator alone. The activator has little effect on the kinds of hydration products.
Key words:fly ash;cement;activator;hydration properties
點(diǎn)擊圖片進(jìn)入活動(dòng)官網(wǎng)預(yù)約參會(huì) >>
>> 相關(guān)內(nèi)容
- 低品質(zhì)粉煤灰的活性激發(fā)研究 (點(diǎn)擊:14351 次)
- 廢石膏粉煤灰石灰結(jié)合料的研究 (點(diǎn)擊:14380 次)
- 粉煤灰和礦渣影響混凝土碳化的因素及建議 (點(diǎn)擊:15723 次)
- 粉煤灰、礦粉復(fù)合雙摻在大體積混凝土配合比中的應(yīng)用 (點(diǎn)擊:19953 次)
- 劣質(zhì)粉煤灰對(duì)混凝土性能的影響探討 (點(diǎn)擊:20196 次)
- 【技術(shù)交流】煤矸石材料填筑路基施工研究 (點(diǎn)擊:15051 次)
- 粉煤灰水熱合成沸石分子篩的研究進(jìn)展 (點(diǎn)擊:23606 次)
- 燃煤灰渣作為混凝土摻合料的新變化及其影響(原創(chuàng)) (點(diǎn)擊:24043 次)
- 高鈣粉煤灰對(duì)混凝土的影響討論 (點(diǎn)擊:21281 次)
#
最新技術(shù)資訊
更多>>- 國(guó)家力推!全固廢免燒膠凝技術(shù)入選國(guó)家重點(diǎn)推廣的低碳技術(shù)目錄,2025上海固廢論壇重磅...
- 2025第二屆中國(guó)(江西)國(guó)際綠色礦業(yè)博覽會(huì),即將盛大開幕!
- 2025第二屆中國(guó)國(guó)際煤炭及礦山技術(shù)裝備展覽會(huì)
- 2025工業(yè)固廢與建筑垃圾綜合利用及工業(yè)污泥協(xié)同處置戰(zhàn)略合作論壇邀請(qǐng)函
- IE expo China 2025第二十六屆中國(guó)環(huán)博會(huì) 亞洲旗艦環(huán)保展,環(huán)保企業(yè)多維提升的平臺(tái)沃土...
- 【技術(shù)分享】助力“雙碳”目標(biāo),響應(yīng)低能耗綠色建筑趨勢(shì),一種粉煤灰及其它固體廢渣復(fù)...
- 一種利用固體廢渣制備人造砂子、石子、砂粉料的制備方法
- 粉煤灰“超細(xì)活化”成建筑新資源
- 關(guān)于粉煤灰循環(huán)利用的發(fā)明專利
- 循環(huán)利用粉煤灰的發(fā)明專利